Eng-Tips is the largest forum for Engineering Professionals on the Internet.

Members share and learn making Eng-Tips Forums the best source of engineering information on the Internet!

  • Congratulations JStephen on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Drawing note with quotes

Status
Not open for further replies.

Dale_Youngs

Aerospace
Joined
Nov 19, 2024
Messages
9
I have an old drawing with a note that specifies the heat treatment of the part. Part of the information is in quotes - "H900". Does anyone know what quotes mean in a drawing note?
 
Op
Is there an other note that specifies heat treat spec.
 
The problem is the rest of the note gives some conflicting requirements in a hardness range and a BAC spec. I cant find any interpretation of quotes in a note that would indicate it would be reference or guidance, but I suspect it was the intent. The problem is that the drawing is so old I cant ask what the intent was.
 
Op
The spec must specify the heat treatment and hardness. Regardless
If it is old ask customer engineering to clarify. Do not guess.
Parenthesis is reference. I believe it was on an old military spec.
 
Thanks, just wanted to make sure I wasnt missing an old convention.
 
Poster is seriously skimpy on info.

Obviously H900 is SStl PHT. There should be a general note or reference on the drawing to a Boeing spec of some kind... in the PL or general notes or 'stock-printed' block somewhere on the drawing face.

WHAT SStl Material/alloy?

/NOTE/ from my days working for USAF: if this is an old Boeing drawing, there may be areas that are illegible... might have to request a checked/verified legible copy of the vellum drawing in the archives.

/CAUTION/ My company no longer allows PHT H900 for 95% of SStl components. H900 = high strength/hardness, low ductility = low fracture toughness and poor SCC resistance. The ONLY exceptions I'm aware of are for parts in pure bearing/compression, like bushings and bearing races.
 
Last edited:
mfg... RE OP post #3...

Mentions 'BAC'... suggests this is a Boeing drawing.

AMS2759/* would likely not apply. However, MIL-H-6875 might apply... if drawing is old-enough.
 
My background is not structural so take my point with a grain of salt. You have probably already reviewed this, but MMPDS-15 Chapter 2 for Steel gives some information about H900, though it does not detail the exact process. It also supports Wil's CAUTION comment about fracture toughness.
 
Do you have access to any of the purchasing and quality information that might go along with the drawing to get the parts? This could be PO's, supplier drawings, materials test cert's, heat treatment cert's, etc. You might at least be able to revise the drawing to reflect the present status of the parts. It can be a little embarrasing to call a supplier and ask what exactly you are buying from them, but sometimes that's how it is.
 
Status