Nov 16, 2007 #1 Armstrong82 Petroleum Joined Nov 16, 2007 Messages 1 Location GB In the field 7" GRP pipe is used, we are doing corrosion tests simulating this pipe. We are using 3.5" pipe. Would you foresee scalability issues? If so what would they be?
In the field 7" GRP pipe is used, we are doing corrosion tests simulating this pipe. We are using 3.5" pipe. Would you foresee scalability issues? If so what would they be?
Nov 17, 2007 #2 EdStainless Materials Joined May 20, 2004 Messages 16,388 Location Waukesha WI USA The only things that come to my mind are matching the temperature gradient through the wall and matching the stress condition. Upvote 0 Downvote
The only things that come to my mind are matching the temperature gradient through the wall and matching the stress condition.