Hello, I have some doubts about some concepts, maybe very basic, but I hope you can help me.
I know that hot spot is a method to eliminate peak stress, normally from the weld toe to evaluate fatigue in S-N curves that do not require this component, but I have also seen this method used in shell geometries for, for example, bolt holes.
Is this correct?
It is my understanding that in shell elements there is no peak stress, since they linearize the stresses directly through the thickness, so a method like the one described in ASME Sec VIII Div 2 does not make sense to eliminate this stress component.
But what about the hot spot method, which linearizes in the meridional or hoop direction? Obviously the stress distribution will not be linear if we apply this method in a bolt hole for example, where there will be a stress concentration.
Is it correct to assume in that case that the stress above the linearized maximum stress at the edge of the hole is a peak stress, and therefore should be eliminated for fatigue analyses that require them?
Thanks in advance
I know that hot spot is a method to eliminate peak stress, normally from the weld toe to evaluate fatigue in S-N curves that do not require this component, but I have also seen this method used in shell geometries for, for example, bolt holes.
Is this correct?
It is my understanding that in shell elements there is no peak stress, since they linearize the stresses directly through the thickness, so a method like the one described in ASME Sec VIII Div 2 does not make sense to eliminate this stress component.
But what about the hot spot method, which linearizes in the meridional or hoop direction? Obviously the stress distribution will not be linear if we apply this method in a bolt hole for example, where there will be a stress concentration.
Is it correct to assume in that case that the stress above the linearized maximum stress at the edge of the hole is a peak stress, and therefore should be eliminated for fatigue analyses that require them?
Thanks in advance