dshiel
Industrial
- Mar 22, 2002
- 4
I work in a Paper Mill and one of our Fan Pumps Has developed high vibration readings. The Pump is a Goulds Double Suction Centrifugal Pump 3400 series. It has a Paraflex Coupling. The Pump runs at 1770 RPM. In the past month we have developed high vibration in the pump. Most of the vibration shows up as 1x. The running element was changed out twice and the pump still has the high 1x vibration with little difference noted between running elements. Readings are as follows in veloscity: Motor- MAH.0625ips, MBH-.0941ips, Pump- PCH-1.22ips 6.6ge PCV- .53ips 6.6ge, PDH- .49ips 9.4ge, PDV- .16ips 6.4ge, PDA-.74ips 8.0ge. The FFT's show a large 1x spike and a small 2x spike. Phase readings showed 171'. Recently, last two days, the Paraflex Coupling Insert failed. Does anyone have any ideas of what is causing this vibration to suddenly occur and continue even after changing the running element????