Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Double Lap Shear Analysis

Status
Not open for further replies.

jonhoward

Mechanical
Oct 12, 2005
6
In the double lap shear case of a bonded joint can someone tell me the analysis standard. Basically, I am wondering if the equation is:

sig= (P)/(lxw) or

sig= (P)/(lxwx2)

if anyone can provide some guidance it would be very helpful!
 
Replies continue below

Recommended for you

Total area of glue being sheared is indeed 2*l*w, so

average_shear_stress = total_load /(2 * bond_length * bond_width)

Test standard ASTM D 3528 might help with the basics.

Note that the average shear is less than the peak shear in the glueline (unless the substrates are very thick, such as in Ray Krieger's KGR adhesive shear measurement machines).

Also note that a good adhesive will have quite a bit of plasticity before it fails. It depends a lot on what you're bonding with what.
 