We have a cast aluminum plate about .55" thick that we have Double Disk ground to get nice parallel sides. Occasionally one side won't clean up. The grinder says the parts are bent too much. The foundry says they're fine. My question is: Can you control how much stock is taken from each side when Double Disk grinding? Or is the same amount taken from each side?