Sep 29, 2020 #1 Joe Chen New member Joined Oct 21, 2016 Messages 19 Location TW Dear All Due to the inner diameter (340 mm) of the bushing is required in the post-lathe process, how long does the liquid nitrogen shrinkage fitting installation need to stress relieve before precision machining to the finished size.
Dear All Due to the inner diameter (340 mm) of the bushing is required in the post-lathe process, how long does the liquid nitrogen shrinkage fitting installation need to stress relieve before precision machining to the finished size.
Sep 29, 2020 #2 JJPellin Mechanical Joined Oct 29, 2002 Messages 2,195 Location US What are the materials involved? Some materials will take a permanent dimensional change if cooled in liquid N2. Johnny Pellin Upvote 0 Downvote
What are the materials involved? Some materials will take a permanent dimensional change if cooled in liquid N2. Johnny Pellin
Sep 29, 2020 Thread starter #3 Joe Chen New member Joined Oct 21, 2016 Messages 19 Location TW The material is SS41. Upvote 0 Downvote
Oct 7, 2020 #4 hydtools Mechanical Joined Apr 4, 2007 Messages 3,265 Location US There will remain internal stress at long as there is an interference fit. Ted Upvote 0 Downvote