Are there any competitors for Domex 100XF? For my purposes (welded structural components of machinery and equipment) it is really awesome stuff!

Here are the specs I am concerned with:

100 ksi yield
10% or better elongation
no heat affected zone when welding
no preheat or post heat needed when welding
1.8t bend radius (low on my priority list)

Thanks!
 
Replies continue below

Recommended for you

There are competitors for 100 ksi yield steel in the USA. Here are two places that specialize in this product:




Depending on the quantity you need, you may want to contact some other suppliers of steel in coil form:



 
TVP, that TP100 looks like it's exactly what I am looking for. Thanks!
 