Jul 21, 2004 #1 pardal Automotive Joined Oct 17, 2001 Messages 444 Location AR I had notice of applying vacuum on Zamac inyection molding of piece. Where I can find more info about it. I did a search with no results. Pardal
I had notice of applying vacuum on Zamac inyection molding of piece. Where I can find more info about it. I did a search with no results. Pardal
Jul 22, 2004 #2 TVP Materials Joined Apr 12, 2002 Messages 4,592 Location US Are you talking about metal injection molding or high pressure die casting? Either way, I am not aware of any company that uses vacuum with either of these processes when zinc is the material. Upvote 0 Downvote
Are you talking about metal injection molding or high pressure die casting? Either way, I am not aware of any company that uses vacuum with either of these processes when zinc is the material.
Aug 16, 2004 Thread starter #3 pardal Automotive Joined Oct 17, 2001 Messages 444 Location AR It is high pressure die casting. Pardal Upvote 0 Downvote