matay
Mechanical
- May 17, 2003
- 12
Hi,
We have a vertical pressure vessel with skirt.Vessel material is SS304 but skirt is SA51670 with 20 and 30mm thk. subsequently.Shell&heads do not need heat treatment but should I heat treat the skirt material? I'm looking at UCS-56 yes it needs but this part is nonpressure part? Can anyone help me about it?
We have a vertical pressure vessel with skirt.Vessel material is SS304 but skirt is SA51670 with 20 and 30mm thk. subsequently.Shell&heads do not need heat treatment but should I heat treat the skirt material? I'm looking at UCS-56 yes it needs but this part is nonpressure part? Can anyone help me about it?