I am having trouble getting an epoxy grout to come to design strenth The material is conditioned for a hot weather pour What about the high humidity in the part of the country where the pour is occurring (SW VA/East TN) The grout is achieving 2000 psi less than jobsite engineering spec and nearly 5000 psi less than the grout supplier spec. Any ideas?
 
Better get the grout supplier involved. These grouts can be tricky, and sometimes bad batches occur.
 
Agree with Hokie... high humidity usually doen't cause a problem with epoxy grouts... temperature, however, can...

Dik
 
Grout mfg is on site Breaks are 1/2 of what they should be Core samples being taken and analyzed of product in place Everything proper and according to C 579 B (molds; cure time; transport; etc.) All at a loss, especially grout mfg Maybe product exceeded shelf life? Sat in a cold warehouse too long (bad winter here-3 weeks of no power)? Air temp has been in the 90s during day, mid 70s at nite - well within range. Any ideas out there?
 