Can anyone help me with the DIN Standard number for Stellite 6R? Cheers, Torsten.
 
The Deloro Stellite website listed the following specifications for Stellite 6:

SAE AMS 5387
SAE AMS 5373
AWS 5.13 RCoCr-A
UNS 30006

I am not aware of any DIN norms that cover cobalt-based alloys. I will perform a search and let you know if I find anything. In the meantime, you may try contacting someone at Deloro Stellite with this question. The website is
 
Thank you for your answer and your help...I am really struggling here...we use Stellite coated wedges within our equipment and I am having a German customer, who is insisting on being told the DIN standard number for this and I just can't get it anywhere...Cheers (from Liverpool), Torsten.
 