In a valve data sheet I found ZCMS 66 specified as seat and spring material. I didn't any International standard referring to it. Does anybody know if this is a specific manufacturer standard or what it is? Thanks.
 
Replies continue below

Recommended for you

I found that "ZCM" may stand for Zinc Composite or Zinc Containing Material; nothing meaningful for "ZCMS"... Is there the possibility of a mispelling, parhaps?

Regards,
'NGL
___________________
 
Zinc Material Safety CAS number 7440-66-6. I would believe they are stating the material coating is Zinc or has Zinc in it, and the safety date sheet Cas Number is 66, Making it ZCMS-66. If I remember right, 66 stand for Molecular weight for ZINC.