I usually call it out something like, "600S162-43 mil @ __ in." In this format, the 600 signifies the depth of 6 inches, the 162 indicates the flange width of 1 5/8" and 43 mil would be the thickness. Then in my notes, I specify the material grades for the different gauges. We also note, "or approved equal" in the notes.