The material P1G1 has certified by supply as following general PWHT simulation test with mill sheet.
If apply ASME SEC.VIII DIV.2, the material P1G1 perform PWHT as following as table 6.16 (reducing temperature and increase holding time),
should we recertificate this material by simulation test piece?

Div.2 had deleted an exemption rule as Div.1 UCS-85(f),
the same material applied between Div.1 & Div.2 is different.
It's so strange.
 