Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations KootK on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Distance between butt weld

Status
Not open for further replies.

dungun

Mechanical
Dec 30, 2005
39
Hi
Is it any restriction in codes that required minimum distance between butt welded for ASME 31.3 code.If any what is the rules?.

 
Replies continue below

Recommended for you

I presume you are referring to proximity of butt welds in pipe. This question has been asked several times. The answer is the Codes do not provide specific guidance. In this situation, use engineering judgment, such as locate the butt welds as far away as possible to avoid overlapping weld heat affected zones and stress concentration effects.
 
What does your WPS say? Use the qualifcation of the procedure as a tool. If this is for root gap.

Review SecIX QW-250.

Talk to a good Welding Eng.as it could be dependent on process.

If this is for proxmity of joints to one another there could be other concerns--again the Welding Eng. could help you.
 
dungun,
If you are refering to the proximity of one butt weld to another then do a search on "Proximity of welds" as this has been asked before.
 
For girth weld spacing, a criterion that was developed many years ago based on welding tests is: the greater of 2 inches or 4 times the wall thickness.
 