I need to weld a P1 material to a P1 material (Pipe), which is relatively straight forward, However, this joint is backed with a stainless steel nozzle, which in effect acts as a backing bar as the root is open. The root run actually holds the nozzle in place within the pipe. I am contemplating putting the first 2 passes in with a 309 consumable then completing the joint with Carbon Steel electrodes. Is this acceptable for B31.1 and B31.3 specs? I already have WPS's for P1 to P1 and P1 to P8. Would a new PQR need to be run? If a PQR is run should the SS backing bar be removed before sending to the Test House?
Any Help would be greatly appreciated.
Many thanks