Subject: ASME Section IX-2013; QW-403.6 - Qualified Base Metal Thickness with
File No: 14-1618
Background: A SMAW procedure qualification test coupon consisting of two plates with the same P-Number
but different Group numbers, and of different base metal thicknesses is groove welded. The
thinner plate, T1 = 0.24 in. thick, and the thicker plate, T2 = 3/8 in. thick. Impact testing is required.
Question (1): Does this test coupon qualify the WPS for a base metal thickness range of 0.120 in. to
0.75 in.?
Reply (1): No.
Question (2): Does this test coupon qualify the WPS for a base metal thickness range of 0.120 in. to
0.480 in. for the T1 Group Number, and 0.375 in. to 0.75 in. for the T2 Group Number?
Reply (2): Yes.
Bckground
Same above topic is similar to my query when applicable impact as per B31.3(range T/2 to T+6 mm ),specifically when its required on weldolet to Runner pipe welding with dissimilar thickness.
Thanks in advance..
Regards,
QC7
Can I get ASME SEC IX interpretation number of below subject,which was discussed and closed in previous thread 292-370252.
DonRoss (Mechanical)
(OP)
1 Dec 14 13:53
Gents,
I wanted to follow-up with my response from ASME.
It hasn't been given an Interpretation number yet.
Subject: ASME Section IX-2013; QW-403.6 - Qualified Base Metal Thickness with
File No: 14-1618
Background: A SMAW procedure qualification test coupon consisting of two plates with the same P-Number
but different Group numbers, and of different base metal thicknesses is groove welded. The
thinner plate, T1 = 0.24 in. thick, and the thicker plate, T2 = 3/8 in. thick. Impact testing is required.
Question (1): Does this test coupon qualify the WPS for a base metal thickness range of 0.120 in. to
0.75 in.?
Reply (1): No.
Question (2): Does this test coupon qualify the WPS for a base metal thickness range of 0.120 in. to
0.480 in. for the T1 Group Number, and 0.375 in. to 0.75 in. for the T2 Group Number?
Reply (2): Yes.
Bckground
Same above topic is similar to my query when applicable impact as per B31.3(range T/2 to T+6 mm ),specifically when its required on weldolet to Runner pipe welding with dissimilar thickness.