Sep 7, 2002 #1 ControlConcepts Electrical Joined Sep 2, 2002 Messages 30 Is the a place where you can see where diferrent metals react with each other. Like what metals to not use on aluminum etc
Is the a place where you can see where diferrent metals react with each other. Like what metals to not use on aluminum etc
Sep 8, 2002 #2 mohtogh Chemical Joined Feb 21, 2001 Messages 144 Location CA What you are seek for it, named "galvanic series ".The most important galvanic series is for sea water.A simple galvanic series, is here: //http://www.allzinc.com/tech/table3.htm That means:In each couple of contacted metals(or alloys) ,higher metal corrode.hope this help you. Upvote 0 Downvote
What you are seek for it, named "galvanic series ".The most important galvanic series is for sea water.A simple galvanic series, is here: //http://www.allzinc.com/tech/table3.htm That means:In each couple of contacted metals(or alloys) ,higher metal corrode.hope this help you.
Sep 8, 2002 #3 mohtogh Chemical Joined Feb 21, 2001 Messages 144 Location CA Another good site, specially for Aluminum, is here : http://www.finishing.com/Library/pennisi/corrosion.html Upvote 0 Downvote
Another good site, specially for Aluminum, is here : http://www.finishing.com/Library/pennisi/corrosion.html