We have to do a weld procedure qualification according to ASME IX: A352 LCC with A pipe 316L.For that, we think that we can find a pipe with similar grade as ASTM A333 Gr6.ASTM A 333Gr 6 is for low T°,and we have a weld with different PNbs 1 groupe 2 and 8 groupe 1, we think we can use a rod for the root and an electrode for following layers , material type SFA 5.4 or 5.9 E 309L AND er 309L which are normally ok for welding carbon steel and 316L.The Probleme is we have to do impact tests according ASME ( - 45°C), and rod and electrode 309L have not impact tests in the material data sheet and pipe are 21.3mm * 2.77mm with 2.77mm thickness we can't do samples for impact test.
Please could you help us and give the way.