MechEgrBDJ
Mechanical
I currently have a project where we are welding 304 ss and 316 ss to carbon steel. This is a lower temp application so I specified a WPS with 309 filler. After PMI on several of the weld it was discovered the wire was marked 309 but was actually 316 ss. What potential problems do I have with these welds?