Would the following chemicals be safely disposed of when used as water to mix with cement and aggregate to make concrete?
Nitric Acid S.G. 1.4 (10ml)
0.1 mol Silver Nitrate Solution (20-25ml)
0.1 mol Potassium Thiocyanate Solution (20-25ml)
Ammonium Ferric Sulphate (1ml)
3,5,5 Trimethyhexanol (2ml)
N.B. These chemicals are used in a Chloride ion titration test for concrete. The amounts used per test are in parentheses.