valvesarefun
Materials
Hello All,
I am wondering if the ferrite present in most CF8M castings helps it to resist chloride induced SCC better than it's wrought counterpart 316SS. I am thinking that its probably too small of a ferrite to austenite ratio to matter, or if it does make a difference then the difference is negligible, but I am interested in getting an authoritative opinion on the subject.
Best Regards,
VRF
I am wondering if the ferrite present in most CF8M castings helps it to resist chloride induced SCC better than it's wrought counterpart 316SS. I am thinking that its probably too small of a ferrite to austenite ratio to matter, or if it does make a difference then the difference is negligible, but I am interested in getting an authoritative opinion on the subject.
Best Regards,
VRF