subsearobot
Mechanical
We are comissioning a mobile hydraulic system, ~65 hp. We have an onboard pump with 6 micron filter on the pressure sied, and 12 on the return. Most of the plumbing is seamless 316. some hose is used too. we are independantly driving up to 7 hydraulic motors using pressure control valves(with no load in testing and flushing).
we also have driven the vehicle's system with a new "bench top" HPU. this unit has the same filtering as the vehicle, with the addition of a 5 micron and water filter, and a 3 (not sure it's absolute though) micron spin-on.
We not loaded the system. we have flushed, changed fluid, and tuned valves a bit - a few hours total.
So, I pulled off a manifold cover that had pockets facing up. the pockets served like setting ponds in the bottom of your resivoir. there was a film of shiny metal "dust" covering the surfaces. they sort of looked like silt or even clay sized particles. We checked varoius points in the system (including filter resivoirs) and found this pixie dust in the oil everywhere. the strange part is that this stuff is not magnetic.
Two questions:
1. do we need to worry? have we endangered our valves?
considering we have so much filtration, this stuff must be smaller than our filtration goal (10 micron abs).
2. where did this glitter come from?
we also have driven the vehicle's system with a new "bench top" HPU. this unit has the same filtering as the vehicle, with the addition of a 5 micron and water filter, and a 3 (not sure it's absolute though) micron spin-on.
We not loaded the system. we have flushed, changed fluid, and tuned valves a bit - a few hours total.
So, I pulled off a manifold cover that had pockets facing up. the pockets served like setting ponds in the bottom of your resivoir. there was a film of shiny metal "dust" covering the surfaces. they sort of looked like silt or even clay sized particles. We checked varoius points in the system (including filter resivoirs) and found this pixie dust in the oil everywhere. the strange part is that this stuff is not magnetic.
Two questions:
1. do we need to worry? have we endangered our valves?
considering we have so much filtration, this stuff must be smaller than our filtration goal (10 micron abs).
2. where did this glitter come from?