As TVP said, 1.4305 is free austenitic free machine grade as AISI 303.
DIN 688 could be a mistake. Right could be DIN 668 ( pemissible variation in size of cold finished bars - i.e cold drawn, centerless ground or peeled and reeled bars ) Tollerance : h 11 ( for instance : round 1" inches , over zero /minus 0,13 millimeter )
Today this DIN 668 is obsolete and was substituded by EN 10278.