I have been recommended for DIN H2 wide standard no 1.0425 for the fabrication of chimmney having temp around 350debg cent.Can anybody recommenmd me the welding electrode for the same.CAn anybody let me know what are the equal standards for the Indian or American community.

Regards
 
Material 1.0425 is named DIN 17155 HII
ASTM similar materials are A414 Gr. E and A516 Gr. 65
Depending on thickness and requirements regular low carbon steel electrodes should be adequate.

 