DIN 17100

Status
Not open for further replies.

martensiticz

Materials
Jul 19, 2009
7
IS DIN 17100 STILL APPLICABLE?
 
Replies continue below

Recommended for you

It is not neccessary to post the same question in 3 different forums. Or are there even more than 3?
 
i am so sorry ,i thought it two times failed to send.

thanks for your appreciated reply
 
martensiticz

That specification, as OSIRIS7 point out is no longer specified in contracts in Europe. But if you have a copy, keep it (I keep mine). Because most older buildings used it in Europe. It was the best in Europe.

And it is the major contributing document to the new EN10025. Steels described in DIN 17100 have same properties now listed in EN 10025. What has changed is the format mostly.

For newer works, use EN 10025.
 
Status
Not open for further replies.