Hi Guys,

I am doing a simulation analysis with Solidworks 2012, of a screw joint, trying to understand the effect of the torque to the material (ultem-1000) which is below the screw head and the washer, because the material is cracking just when the torque is applied.

I am using a bolt connector made of 316 SS, and a washer which uses the same material, so when I run the simulation, the results are very high using the bolt connector. However, if I utilized a compressed axial force of 133.33 lbf and a torque of 1.6 in-lbs respectively, the results are very low. I am concerned about the difference of using bolt connector and applying external forces.

Could you please help me to understand the differences?

Thanks in advance.

Esteban
 
Is the Ultem part made with the glass-reinforced variety? Depending on the quantity of glass, it gets very brittle. Like, only a few % elongation (or contraction if the compressive modulus is similar) before break. I have no trouble believing that a metal screw can crack a plastic part. Depending on the size of that screw it could be installed with more than 10x the torque you're trying to use.

-datasheet-


STF
 
Hi SparWeb,

The material does not have any glass. Here's the datasheet I received it from the material directly. Also, The size of the screw is #0-80, the torque is 1.6 in-lbs
However, my concern is about the compression force which is been applied when the torque is applied. By hand I am using the formula T=0.2*D*F to calculate the axial force, which is around 133.33 lbf, using this value the stress is around 39 Ksi (133.33 lbs/3.389x 10-3 in^2), because the area I am assuming is under stress is the circular ring behind the flat washer. So, according to this, the stress is exceeding the compressive force and I got it, which is only 22 ksi.

However, my effort is to reference my hand calcs with the static FEA simulation from solidworks. I started using threaded connectors and the results are 52 ksi for Von Mises Stress, which is higher than my values with hand calcs. Thus I tried using a compressive force equal to the axial force on the washer surface and is giving me higher values (84 Ksi) and then I tried the torque as an external force and it goes down but higher than using connectors (64 Ksi).

I am not sure which one I have to believe. Also as this is a very brittle material, I thought in using non-linear would help and I did it, so I could define the stress-strain curve, but my results change with the time I applied the torque, so I do not know what is the best time which could give me realistic results.

Thanks.

 
 http://files.engineering.com/getfile.aspx?folder=95785497-5d6d-4cae-aea5-d397ee953f1a&file=ULTEM_1000_datasheet_from_Inoplas.pdf