I need to find the difference between ASTM A284 Grade C and Grade D?
 
Replies continue below

Recommended for you

ASTM A 284 was Withdrawn and Replaced by ASTM A 283. I don't know if the Grades are the same between the specifications, so you may have a problem if you have a historical part and need to know its properties. If it is for a new application, then just use A 283.

Regards,

Cory