As per API 600 table 1,there are different trim types.
As you can see in attached file,trim 10&13 have different chemical composition,different mechanical properties and
of course different application.
Trim 10 and 13 are completely different. API Trim 10 calls for 316 on all internal parts (seat, disc, backseat and stem), whereas API Trim 13 does the same, but the material is Alloy 20. Stainless steel grade SS316 has a broad range of applications, but Alloy 20 is often used in sulphuric acid applications with high concentration; at times Alloy 20 valves are substituted with Uranus B6 valves.