Can somebody tell me the difference between a Roll Tap and a normal Tap. Does a roll tap not produce swarf. I've read that somewehere but surely some swarf has to be present or else there would be no thread??

God bless,

Phil.
 
Replies continue below

Recommended for you

A roll tap does not produce swarf. It produces the thread by pushing some material in (to make the root/major diameter on an internal thread), which causes other material to flow out to make the crest/minor diameter.

Regards,

Cory