Can i know the difference from point of view of thermal expansion & the role of different compositions.
Basically we are checking our exsiting superheater for new superior materials.
In general i know for higher grades the thermal conductivity decreases and the elasticity gets better(due to addition of alloying elements).
Design Temperature of flue gas in shell: 1400 deg C
Steam water temperature in tubes is ~ 500 deg C
Following are materials
1. SA-213 T12 Vs SA-213 T22 - TUBES
2. SA-335 P12 Vs SA-335 P22 - HEADERS
3. SA-209 T1 Vs SA-234 WP 91 - BENDS
and we are checking superior grade i.e. SA-213 T22 , SA-335 P22 and SA-234 WP 91 against existing materials i.e. SA-213 T12 , SA-335 P12 and SA-209 T1 as the existing materials are causing sagging of tubes.
Appreciate your fast response, please
Its urgent.
Osama
Osama Nusrat Ali
Basically we are checking our exsiting superheater for new superior materials.
In general i know for higher grades the thermal conductivity decreases and the elasticity gets better(due to addition of alloying elements).
Design Temperature of flue gas in shell: 1400 deg C
Steam water temperature in tubes is ~ 500 deg C
Following are materials
1. SA-213 T12 Vs SA-213 T22 - TUBES
2. SA-335 P12 Vs SA-335 P22 - HEADERS
3. SA-209 T1 Vs SA-234 WP 91 - BENDS
and we are checking superior grade i.e. SA-213 T22 , SA-335 P22 and SA-234 WP 91 against existing materials i.e. SA-213 T12 , SA-335 P12 and SA-209 T1 as the existing materials are causing sagging of tubes.
Appreciate your fast response, please
Its urgent.
Osama