On another thread, I was admonished for not knowing what a "Class I" casting is.

It was in reference to a question on a die cast part out of ADC12 (A383).

I explained we use NADCA standards for specifications, which is parameter specific (i.e. surface finish, linear tolerance, etc. all get their own class spec) as opposed to one overarching "class".

I'm genuinely curious what standard the other user is referring to.
 
Replies continue below

Recommended for you

AMS2175

"Hoffen wir mal, dass alles gut geht !"
General Paulus, Nov 1942, outside Stalingrad after the launch of Operation Uranus.
 
Thanks @rb1957 - good bedtime reading!
 
yep, it'll surely put you to sleep. pleasant dreams ...

"Hoffen wir mal, dass alles gut geht !"
General Paulus, Nov 1942, outside Stalingrad after the launch of Operation Uranus.
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor