Dear all,

some days ago speaking with friend works in automotive industries I found out Telene Material.
have you got some technical info about Telene? Do you think it could be used in a chemical plants instead teflon?
Have you got permeability values?
 
Replies continue below

Recommended for you

have you got some technical info about Telene?
Contact Demeta for information about NexTene.

Do you think it could be used in a chemical plants instead teflon?
Don't as PDCPD and PTFE have defferent properties and applications.

Have you got permeability values?
As I know permeability depends on catalyst and conditions during polymerization. Ask Vendors for details.
 