I am trying to find the equation for the amount of weight-sag in a large round carbon-steel horizontal cylinder. If a cyl. is round when its axis is vertical, the diameters will change when the axis is horizontal and the bottom of the cyl. is on the floor (cyl. will become shorter vertically and wider horiz.). In my specific case we are making cylinders that are 4675 mm in diameter (OD), from 32 mm thick plates.
I don't think the length of them is a factor-just the wall thickness, dia. and E.