mapleleafs
Civil/Environmental
Has anyone experienced dezincification of pump impellers? We started our water treatment plant 5 years ago and now have to replace all our impellers on are vertical turbine pumps. The original material was a brass alloy 875 ( 15% Zinc ) and the manufacturer is recommending a Tin Alloy 903. We are also trying to find out why this occurred. Are water at the time of startup would have been ph 6.8 and have a chlorine residual of 1.0 mg/l free. The water is low in alkalinity ( 10 mg/l ) It appears that the damage was done in the first two years as the flows had dropped off by 12% during this time. We started using a zinc polyphosphate for corrosion control after the 2 years and pump production stayed the same as if the damage stopped occurring. Any comments would be appreciated.