I have a specimen of Ti-6Al-4V plate (approx. 3" x 3" x 5" with the grain in the 5" direction). I need to determine the 9 orthotropic properties (3 Young's moduli, 3 shear moduli, 3 Poissons ratios). However, I don't want to alter the specimen (e.g., for tensile tests). Can the orthotropic properties be determined by measuring the wave speed in the three directions with ultrasonic pulse echo? If so:
- Who could perform these tests?
- Where can I find literature that gives details and limitations of this test?
Are there other non-destructive tests that would give the properties?
Thanks,
Don Culp
- Who could perform these tests?
- Where can I find literature that gives details and limitations of this test?
Are there other non-destructive tests that would give the properties?
Thanks,
Don Culp