Could anyone tell me the meaning / significance of the letters SA in the designation of ASME/ASTM specifications?

e.g. SA 516.

Regards,
Quadswift
 
Replies continue below

Recommended for you

SA is the ASME prefix for the A in ASTM designators.
 