Jul 22, 2003 #1 quadswift Petroleum Joined Nov 7, 2002 Messages 39 Location GB Could anyone tell me the meaning / significance of the letters SA in the designation of ASME/ASTM specifications? e.g. SA 516. Regards, Quadswift
Could anyone tell me the meaning / significance of the letters SA in the designation of ASME/ASTM specifications? e.g. SA 516. Regards, Quadswift
Jul 22, 2003 #2 Metalguy Materials Joined Jan 2, 2003 Messages 1,412 Location US SA is the ASME prefix for the A in ASTM designators. Upvote 0 Downvote