I routinely perform tensile testing using specimens with either a 1.0" gauge length or a 2.0" gauge length (both 4D type specimens, ASTM E8-24). Often, in reporting my results, I am asked to specify the manufacturer's acceptance criteria (min allowable) along with my test results. For % Elongation, I report the gauge length of the specimen with the % Elongation results. However, the manufacturer's acceptance criteria for % Elongation is often provided specifically for a 2.0" gauge length. In those cases, I go ahead and report my test results and state the gauge length of the specimen. My question is this: what are your thoughts on reporting a % Elongation from a 1.0" gauge length specimen and comparing it to an acceptance criterion based on a 2.0" gauge length? If both specimens are ASTM E8 4D specimen types, should it matter? Should I simply be reporting my % Elongation results and stating "4D specimen"? Thanks.
 
Last edited:
Is this all just ASTM work?
If so then just report it as 4d and move on.
I have had the other issue, AMS specs that require 2" gage length and parts that only 0.1375" in diameter.
It is very difficult to meet elongation in that situation.
 
Is this all just ASTM work?
If so then just report it as 4d and move on.
I have had the other issue, AMS specs that require 2" gage length and parts that only 0.1375" in diameter.
It is very difficult to meet elongation in that situation.
Yes - the tensile testing is all ASTM work. Thanks for the advice.
 
Since you are testing both gage lengths of specimens, you really should select the gage in the requirements to machine and test. If it is impractical, then use the results from the shorter gage length along with a note to the effect that the material still passes but with the caveat that a shorter gage length was tested.
 