For every material there is a specified design pressure and design temperature. Now if i am operating at a pressure less then design pressure, can I go on operating at higher than design temperature. Example: for a refractory lined killed carbon steel design pressure is 4.4 Kg/cm2 (g) and design temperature (internal) is 742 deg C. Now I operate at around 3.6 kg/cm2 (g)then can I have operating temperature more than 742 deg C say 750 deg C.