asirana

Materials
Jun 24, 2015
1
Hi all,
Can any body guide me on how and where to fine maximum allowable working (Design temperatures) for various metals/materials like carbon steel plates and pipes, SS 300 series plates and pipes and so on.
Also for cast iron materials etc.
does any body have a list for quick reference?
Appreciate your quick response.
 
Replies continue below

Recommended for you

Matweb. Also most mill data bulletins or tech sheets are going to contain this information. If both of these fail to yield the information you need, a good, experienced metallurgist should be able to help.

It is better to have enough ideas for some of them to be wrong, than to be always right by having no ideas at all.
 
If you are talking about design limits then you need to check ASME B&PVC.
If you are just talking about application limits then use reference books, manufacturer data sheets, and other such sources.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 
Depends upon the property you're looking at designing against ornerynorsk.

The advice above is spot-on.

eg: if it's a beam in a walking beam furnace, max service temp = 300C. If it was scale resistance, it'd be higher and dependent upon composition.
 