We have a client that begs us not use steel even in the landing zones of heavy aircraft. In lieu of steel, we thicken the concrete about 20% more. Of course this goes through several calulations and is not a random guess thickness. But the reason the client hates steel is that it is more expensive to install and the service life is same, and demolition is half the costs since there is no steel to deal with. You might consider fiber mesh for driveways. We use fibermesh in many cases and are really amazed how well it holds up.