I have a 35 ft atmospheric tank which shows some dent (inward deformation). Bulge would be a better word but bulge is for outward deformation.
How can I evaluate them for integrity and return in service ? API 579 don't include cylindrical with more than 42 inches diameter...(section 12). Can you help me to find some acceptance criteria ?
Does the fact that dent are inward and tank is only atmospheric pressure (under 16 psi at the bottom)help to not being a big issue here ?
Please discuss
Cedric
How can I evaluate them for integrity and return in service ? API 579 don't include cylindrical with more than 42 inches diameter...(section 12). Can you help me to find some acceptance criteria ?
Does the fact that dent are inward and tank is only atmospheric pressure (under 16 psi at the bottom)help to not being a big issue here ?