I have a situation. I have been testing for 2-days using a VTM-12 (Virginia Test Method) One Point Proctor values of 104.7 lb/cu.ft @19.2 OMC. The VTM-12 test uses Standard effort.
For 2 days I have passed compaction in a green area requiring 85% of Standard Proctor. My lab tech mistakenly ran a modified Proctor yielding values of 115.3 lb/cu. ft @ 14.9% OMC. Obviously, the previous tests no longer meet the 85% compaction required.
I will have him rerun the test, but in the meantime, can anyone give a general %-comp equivalency for 85% and 95% of Standard Proctor? Soil is a sandy CL with negligable gravel.
TIA
For 2 days I have passed compaction in a green area requiring 85% of Standard Proctor. My lab tech mistakenly ran a modified Proctor yielding values of 115.3 lb/cu. ft @ 14.9% OMC. Obviously, the previous tests no longer meet the 85% compaction required.
I will have him rerun the test, but in the meantime, can anyone give a general %-comp equivalency for 85% and 95% of Standard Proctor? Soil is a sandy CL with negligable gravel.
TIA