Hi

I have a question about possibilities implement user-material subroutine included changing material density. I have thermal problem where I should assume diffrent density. I would like implement changing density in every material element and watching strain distribution as a result of diffrent density.
Is it possible in Abaqus? If yes which subroutine i should use.

Thanks for help
 
It depends how your density changes. Is it spatially, i.e. according to position of the elements; or does it depend on position, or both?

If it just depends on temperature then you can do this already in the specification of ABAQUS material properties. If it's a little more complicated you could use field variables perhaps:
 
I think defining density-temperature curve should do the trick :-)

Regards

arrrrrrrrrrrrr!!!
 
Tkanks mrgoldthorpe and Noirom84 for advices. :-)
 