Could any one suggest source to procure demister with 6'-0" diameter x 12 inch thick with 12 lbs/ft3 density at top and 5 lbs/ft3 at bottom. Material SS 304L.

The reduction in density shall be gradual.

Thanks in advance
 
Replies continue below

Recommended for you

I've seen this done in 3 separate sections. Try Raschig or Koch-Glitsch.
 