Shrinkage of column does not occur until the forms are removed. If there is no removal of form, then the delay interval does not help for column shrinkage effect. If the column forms are removed, then the elevation set for the slab will have to be independent of the column to minimize the column shrinkage effect, (thickening the slab at the location of the column to make up the column shrink).