A urgent question. I designed a factory shed last year, and they are building it now. The rafter is 310UB slope from one end to another, span 20m, with 3m haunch both end. The column is 360UB, high 3.6m at on end, and 5.2m at the other. The rafter rigid connected to the column. There is a bolted splice at the middle of the rafter. (top and bottom flange, web bolts with plate).
Now my problem is, in my calculation, the rafter is deflect 43mm under dead load, but now during constrution, the beam is deflect 30mm only under self weight, So I guess it will deflect more than 80mm under deal load (included purlin and roof sheeting). The owner is not happy about this deflection. Do your guys have any idea to improved the deflection without major change of the design? I think the main reason for this happen is because the bolt splice, in my member design, I consider it as a single beam, but because 310UB not available for 20m long, so I designed a bolt splice at the middle, may be the bolt hole and the bolts create some rotation.
Thank you for your time.
PowerRanger
A urgent question. I designed a factory shed last year, and they are building it now. The rafter is 310UB slope from one end to another, span 20m, with 3m haunch both end. The column is 360UB, high 3.6m at on end, and 5.2m at the other. The rafter rigid connected to the column. There is a bolted splice at the middle of the rafter. (top and bottom flange, web bolts with plate).
Now my problem is, in my calculation, the rafter is deflect 43mm under dead load, but now during constrution, the beam is deflect 30mm only under self weight, So I guess it will deflect more than 80mm under deal load (included purlin and roof sheeting). The owner is not happy about this deflection. Do your guys have any idea to improved the deflection without major change of the design? I think the main reason for this happen is because the bolt splice, in my member design, I consider it as a single beam, but because 310UB not available for 20m long, so I designed a bolt splice at the middle, may be the bolt hole and the bolts create some rotation.
Thank you for your time.
PowerRanger