stillfan1
Structural
- Oct 21, 2019
- 3
I have always been under the impression that if you have a continuous helix shaped transverse bar it was a spiral. Today I had an individual point out that the ACI318-14 R25.7.2.3 states that a circular continuously wound bar or wire is considered a spiral if it conforms to 25.7.3 (volumetric spiral ratio equation) otherwise, it is considered a tie. I thought spirals were ties? And if it is considered a tie, in a round pile, what is the longitudinal rebar spacing requirement. Is it the same as a rectilinear tie, with 6" spacing max unless additional transverse rebar is provided?